• head_banner_01

LLDPE M500026T

Short Description:

SABIC Brand

LLDPE| Injection MI=50

Made In Saudi Arabia

 


  • Price : 1000-1200 USD/MT
  • Port: Huangpu / Ningbo / Shanghai / Qingdao
  • MOQ: 1*40GP
  • CAS No:: 9002-88-4
  • HS Code: 3901402090
  • Payment : TT/ LC
  • Product Detail

    Description

    M500026T is a Linear Low Density Polyethylene grade with narrow molecular weight distribution suitable for injection moldingapplications. It has been designed to give excellent flow properties with better low temperature toughness, stress crack resistance and gloss.

    Typical Property Values

    PROPERTIES TYPICAL VALUES UNITS TEST METHODS
    POLYMER PROPERTIES   
    Density 926 kg/m³ ASTM D1505
    Melt Flow Rate (MFR)   
    at 190℃ and 2.16 kg 50 g/10 min ASTM D1238
    MECHANICAL PROPERTIES   
    Flexural Strength 9 MPa ASTM D790
    Flexural Modulus (1% Secant) 200 MPa ASTM D790 A
    Izod Impact Strength 500 J/m ASTM D256
    Hardness (Shore D) 50 - ASTM D2240
    ESCR (10% Igepal), F50 3 Hrs ASTM D1693B
    ESCR (100% Igepal), F50 6 Hrs ASTM D1693B
    Tensile stress at yield (50mm/min) 10 MPa ISO 527-2 1A
    Tensile stress at break (5mm/min) 12 MPa ISO 527-2 1A
    Tensile strain at break (5mm/min) >100 % ISO 527-2 1A
    THERMAL PROPERTIES   
    Vicat Softening Point 88 ASTM D1525
    Brittleness Temperature <-75 ASTM D746

    Processing Conditions

     Typical processing conditions for M500026T are: Barrel temperature: 180 - 230°C Mold temperature: 15 -60 °C Injection pressure: 600 - 1000 Bar.

    Health And Safety Considerations And Precautions

    M500026T is suitable for Food contact application. Detailed information is provided in relevant Material Safety Datasheet and for additional specific information please contact SABIC local representative for certificate. DISCLAIMER: This product is not intended for and must not be used in any pharmaceutical/medical applications.

    Storage And Handling

    Polyethylene resin should be stored in a manner to prevent a direct exposure to sunlight and/or heat. The storage area should also be dry and preferably do not exceed 50°C. SABIC would not give warranty to bad storage conditions which may lead to quality deterioration such as color change, bad smell  and inadequate product performance. It is advisable to process PE resin within 6 months after delivery.